Polymer Property : Modulus of Rupture = 0.276 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 0.276 - 0.414 GPa
40.0 - 60.0 ksi
Dry
Unifrax Foamfrax® RG Insulation
Foamfrax® RG (Refractory Grade) Insulation is an extension of the Foamfrax Insulation product line. Foamfrax RG Insulation is a combination of refractory ceramic fiber or soluble fiber, refractory..