Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.0300 GPa @Treatment Temp. 954 °C |
4.35 ksi @Treatment Temp. 1750 °F |
fired and cooled |
Pyrotek Pyrocast ALF2 Low Cement Refractory Castable Pyrocast ALF2 is a low cement castable with mullite base. It is suited for applications requiring high strength at elevated temperatures and abrasion resistance.ApplicationsAluminum melting and hol.. |
|||
Modulus of Rupture | 0.0300 GPa | 4.35 ksi | parallel to thickness |
Zircar Refractory Composites RSLE-501 CYLINDERS Refractory Sheet ZIRCAR Refractory Sheet Type RSLE-501 is a low expansion high strength reinforced silica matrix composites in a cylindrical form. This material was designed for use as a high strength, durable insul.. |
|||
Modulus of Rupture | 0.0300 GPa | 4.35 ksi | parallel to thickness |
Zircar Refractory Composites RSLE-57 Refractory Sheet ZIRCAR Refractory Sheet Type RSLE-57 is a low expansion high strength reinforced silica matrix composite . This material was designed for use as a high strength insulator in induction hot press appl.. |
|||
Modulus of Rupture | 0.0300 GPa @Treatment Temp. 954 °C |
4.35 ksi @Treatment Temp. 1750 °F |
fired and cooled |
Pyrotek Pyrocast ALF3 Low Cement Refractory Castable Pyrocast ALF3 is a low cement castable with a high-purity mullite base. It is suited for applications exposed to high erosion or aggressive alloys and/or atmospheres.ApplicationsAluminum melting an.. |