Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.0140 GPa @Treatment Temp. 725 °C |
2.03 ksi @Treatment Temp. 1340 °F |
|
Pyrotek Pyrocast XL Small Component Refractory ApplicationsThimbles Transition plates Down Spouts Control Pins Auto pour Ladles Strip Casting Nozzles AdvantagesThermal shock resistance High erosion resistance High service temperature Smooth cast.. |