Mechanical Properties Metric English Comments
Modulus of Rupture 0.0120 GPa

@Treatment Temp. 540 °C
1.74 ksi

@Treatment Temp. 1000 °F
Pyrotek Pyrocast AR-S Castable Refractory
Pyrocast AR-S is a low cement, fused silica, castable refractory which exhibits excellent resistance to thermal shock. It is inert to liquid aluminum and its alloys. It is a high strength material..