Modulus of Rupture 0.0100 GPa

@Treatment Temp. 725 °C
1.45 ksi

@Treatment Temp. 1340 °F
Pyrotek Pyrocast AR PLUS Castable Refractory
Pyrocast AR Plus is a fused silica refractory castable inert to molten aluminum and its alloys. Parts cast from Pyrocast AR Plus are heat-treated to ensure that free and combined water are removed...
Modulus of Rupture 0.0100 GPa

@Treatment Temp. 725 °C
1.45 ksi

@Treatment Temp. 1340 °F
ASTM C133-84
Pyrotek Pyrocast 220HT Refractory Castable
Pyrocast 220HT is a high-performance refractory castable based on fused silica and silicon carbide.ApplicationsTransfer troughs Launder linings Filter boxes Pins and spouts AdvantagesThermal shock r..
Modulus of Rupture 0.0100 GPa
1.45 ksi
Pyrotek Pyrocast ICL Castable Refractory