Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00352 GPa | 0.510 ksi | Dry Modulus of Rupture, 50% clay/50% flint, cast bars |
Old Hickory Thomas Tennessee Ball Clay Thomas clay is similar to Volunteer clay and has established an excellent history of performance in stoneware and low fire (talc base) plastic and casting formulas. The diverse combination of clays .. |