Mechanical Properties Metric English Comments
Compressive Modulus 0.500 GPa

@Temperature 100 °C
72.5 ksi

@Temperature 212 °F
X direction, Condition A; ASTM D695
Rogers Corporation RT/duroid® 5880 Glass Microfiber Reinforced PTFE High Frequency Laminate
RT/duroid® 5870 and 5880 glass microfiber reinforced PTFE composites are designed for exacting stripline and microstrip circuit applications. Glass reinforcing microfibers are randomly oriented to..
Compressive Modulus 0.500 GPa

@Temperature 100 °C
72.5 ksi

@Temperature 212 °F
Y direction, Condition A; ASTM D695
Rogers Corporation RT/duroid® 5880 Glass Microfiber Reinforced PTFE High Frequency Laminate
RT/duroid® 5870 and 5880 glass microfiber reinforced PTFE composites are designed for exacting stripline and microstrip circuit applications. Glass reinforcing microfibers are randomly oriented to..
Compressive Modulus 0.500 GPa

@Temperature 316 °C
72.5 ksi

@Temperature 601 °F
ASTM D695 Modified
Saint-Gobain Meldin® 2021 Bearing
General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Series ca..
Compressive Modulus 0.500 GPa

@Temperature 260 °C
72.5 ksi

@Temperature 500 °F
ASTM D695 Modified
Saint-Gobain Meldin® 2030 Bearing
General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Series ca..