Mechanical Properties Metric English Comments
Compressive Modulus 24.1 GPa

@Temperature 71.1 °C
3500 ksi

@Temperature 160 °F
Wet; ASTM D695
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Compressive Modulus 24.1 GPa

@Temperature 71.1 °C
3500 ksi

@Temperature 160 °F
Dry; ASTM D695
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Compressive Modulus 24.1 GPa

@Temperature 93.3 °C
3500 ksi

@Temperature 200 °F
Dry; ASTM D695
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Compressive Modulus 24.1 GPa

@Temperature 23.9 °C
3500 ksi

@Temperature 75.0 °F
Dry; 325°F Autoclave Cured; ASTM D695
Park Electrochemical Nelcote® F-502 Phenolic Prepreg, 7781 E-Glass Reinforced
Nelcote® F-502 is a MIL-R-9299 phenolic resin system suitable for impregnation on any MIL-C-9084 fabric with a compatible finish. F-502 is used in the manufacture of ablative reinforcements in rock..
Compressive Modulus 24.1 GPa

@Temperature 23.9 °C
3500 ksi

@Temperature 75.0 °F
Dry; Oven Cure, 90min, 260°F; ASTM D695
Park Electrochemical Nelcote® F-529 Phenolic Prepreg, 7781 E-Glass Reinforced
Nelcote® F-529 is a non-halogenated phenolic resin designed specifically for use in aircraft and mass-transit interior laminate and sandwich panels. F-529 was formulated for applications requiring ..
Compressive Modulus 24.1 GPa

@Temperature 23.9 °C
3500 ksi

@Temperature 75.0 °F
Dry; ASTM D695
Park Electrochemical Nelcote® P-650M Polyester Prepreg, 7781 E-Glass Reinforced
Nelcote® P-650M is a polyester resin system suitable for coating on any MIL-C-9084. P-650M has good electrical and mechanical properties and has been used in a wide variety of applications, includi..
Compressive Modulus 24.1 GPa

@Temperature 149 °C
3500 ksi

@Temperature 300 °F
Wet; ASTM D695
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 4581 Quartz Reinforced
Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp..
Compressive Modulus 24.1 GPa

@Temperature 149 °C
3500 ksi

@Temperature 300 °F
Dry; ASTM D695
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 4581 Quartz Reinforced
Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp..
Compressive Modulus 24.1 GPa

@Temperature -54.0 °C
3500 ksi

@Temperature -65.2 °F
Dry
Hexcel® F161 Epoxy Resin, 120 Kevlar Fabric
Hexcel designation: 120-38"-F161; Fiber: Kev. 49 195Information provided by HexCel