Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 23.4 GPa @Temperature 71.1 °C |
3400 ksi @Temperature 160 °F |
Dry; Oven Cure 250°F, 90 min; ASTM D695 |
Park Electrochemical Nelcote® E-763 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-763 is a modified epoxy system with a nominal 250°F cure temperature. E-763 provides a transparent resin surface on the finished part which gives finished part surfaces a cosmetic attra.. |
|||
Compressive Modulus | 23.4 GPa @Temperature 23.9 °C |
3400 ksi @Temperature 75.0 °F |
Dry; Post-Cure |
Park Electrochemical Nelcote® V-341 Polybutadiene Prepreg, 581 Quartz Reinforced Nelcote® V-341 is Polybutadiene resin system designed to provide excellent electrical properties in demanding airborne, shipboard, and undersea applications.Key Features and Benefits:Extremely low .. |