Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 117 GPa @Temperature 71.1 °C |
17000 ksi @Temperature 160 °F |
0°, Wet |
Hexcel® HexPly® 8552 Epoxy Matrix, AS4 Fiber Information provided by HexCel |