Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 114.5 GPa @Temperature 24.0 °C |
16610 ksi @Temperature 75.2 °F |
Dry |
Hexcel® HexPly® F593 Epoxy Resin, T2G190 Carbon Tape Hexcel designation: T2GXXX-12"-F593; Fiber: Amoco T-300/12kInformation provided by HexCel |
|||
Compressive Modulus | 114.5 GPa @Temperature -59.0 °C |
16610 ksi @Temperature -74.2 °F |
Dry |
Hexcel® HexPly® F593 Epoxy Resin, T2G145 Carbon Tape Hexcel designation: T2GXXX-12"-F593; Fiber: Amoco T-300/12kInformation provided by HexCel |
|||
Compressive Modulus | 114.5 GPa @Temperature 93.0 °C |
16610 ksi @Temperature 199 °F |
Dry |
Hexcel® HexPly® F593 Epoxy Resin, T2G145 Carbon Tape Hexcel designation: T2GXXX-12"-F593; Fiber: Amoco T-300/12kInformation provided by HexCel |