Polymer Property : Compressive Modulus = 58.7 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 58.7 GPa

@Temperature -59.0 °C
8510 ksi

@Temperature -74.2 °F
T300, Plain Weave; Fill Compression
Hexcel® HexPly® F655 Bismaleimide Resin, Carbon Fabric Form
Fiber: T300-3KInformation provided by HexCel