Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 24.1 GPa @Temperature 71.1 °C |
3500 ksi @Temperature 160 °F |
Wet; ASTM D695 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Compressive Modulus | 24.1 GPa @Temperature 71.1 °C |
3500 ksi @Temperature 160 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Compressive Modulus | 24.1 GPa @Temperature 93.3 °C |
3500 ksi @Temperature 200 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Compressive Modulus | 24.1 GPa @Temperature 23.9 °C |
3500 ksi @Temperature 75.0 °F |
Dry; 325°F Autoclave Cured; ASTM D695 |
Park Electrochemical Nelcote® F-502 Phenolic Prepreg, 7781 E-Glass Reinforced Nelcote® F-502 is a MIL-R-9299 phenolic resin system suitable for impregnation on any MIL-C-9084 fabric with a compatible finish. F-502 is used in the manufacture of ablative reinforcements in rock.. |
|||
Compressive Modulus | 24.1 GPa @Temperature 23.9 °C |
3500 ksi @Temperature 75.0 °F |
Dry; Oven Cure, 90min, 260°F; ASTM D695 |
Park Electrochemical Nelcote® F-529 Phenolic Prepreg, 7781 E-Glass Reinforced Nelcote® F-529 is a non-halogenated phenolic resin designed specifically for use in aircraft and mass-transit interior laminate and sandwich panels. F-529 was formulated for applications requiring .. |
|||
Compressive Modulus | 24.1 GPa @Temperature 23.9 °C |
3500 ksi @Temperature 75.0 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® P-650M Polyester Prepreg, 7781 E-Glass Reinforced Nelcote® P-650M is a polyester resin system suitable for coating on any MIL-C-9084. P-650M has good electrical and mechanical properties and has been used in a wide variety of applications, includi.. |
|||
Compressive Modulus | 24.1 GPa @Temperature 149 °C |
3500 ksi @Temperature 300 °F |
Wet; ASTM D695 |
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 4581 Quartz Reinforced Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp.. |
|||
Compressive Modulus | 24.1 GPa @Temperature 149 °C |
3500 ksi @Temperature 300 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 4581 Quartz Reinforced Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp.. |
|||
Compressive Modulus | 24.1 GPa @Temperature -54.0 °C |
3500 ksi @Temperature -65.2 °F |
Dry |
Hexcel® F161 Epoxy Resin, 120 Kevlar Fabric Hexcel designation: 120-38"-F161; Fiber: Kev. 49 195Information provided by HexCel |