Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 21.4 GPa @Temperature 87.8 °C |
3100 ksi @Temperature 190 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® E-722 Epoxy Prepreg, 285 Kevlar® Reinforced Nelcote® E-722 is a modified 350°F cure epoxy system with excellent processing characteristics for vacuum bag, press, and autoclave molding.Key Features and Benefits:Epoxy resin system optimized f.. |
|||
Compressive Modulus | 21.4 GPa @Temperature 71.1 °C |
3100 ksi @Temperature 160 °F |
Wet; ASTM D695 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 120 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Compressive Modulus | 21.4 GPa @Temperature 71.1 °C |
3100 ksi @Temperature 160 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 120 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Compressive Modulus | 21.4 GPa @Temperature 71.1 °C |
3100 ksi @Temperature 160 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 4581 Quartz Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Compressive Modulus | 21.4 GPa @Temperature 177 °C |
3100 ksi @Temperature 351 °F |
0° |
Hexcel® HexPly® 954-2A Curing Cyanate Resin, Quartz Fiber Reinforced 8 Harness Satin Fabric Information provided by HexCel |
|||
Compressive Modulus | 21.4 GPa @Temperature 71.0 °C |
3100 ksi @Temperature 160 °F |
1/2 hr |
Hexcel® HexPly® F515 Epoxy Resin, 7781 Glass Fabric Hexcel designation: 7781-38"-F515; Fiber 75-1/0Information provided by HexCel |
|||
Compressive Modulus | 21.4 GPa @Temperature 177 °C |
3100 ksi @Temperature 351 °F |
|
Hexcel® HexPly® F263 Epoxy Resin, 120 Glass Fabric Hexcel designation: 120-38"-F263; Fiber: 450-1/2Information provided by HexCel |