Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 20.7 GPa @Temperature 87.8 °C |
3000 ksi @Temperature 190 °F |
Wet (2hr water boil immersion); ASTM D695 |
Park Electrochemical Nelcote® E-722 Epoxy Prepreg, 285 Kevlar® Reinforced Nelcote® E-722 is a modified 350°F cure epoxy system with excellent processing characteristics for vacuum bag, press, and autoclave molding.Key Features and Benefits:Epoxy resin system optimized f.. |
|||
Compressive Modulus | 20.7 GPa @Temperature 71.1 °C |
3000 ksi @Temperature 160 °F |
Wet; ASTM D695 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 4581 Quartz Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Compressive Modulus | 20.7 GPa @Temperature 260 °C |
3000 ksi @Temperature 500 °F |
Dry; 325°F Autoclave Cured; ASTM D695 |
Park Electrochemical Nelcote® F-502 Phenolic Prepreg, 7781 E-Glass Reinforced Nelcote® F-502 is a MIL-R-9299 phenolic resin system suitable for impregnation on any MIL-C-9084 fabric with a compatible finish. F-502 is used in the manufacture of ablative reinforcements in rock.. |
|||
Compressive Modulus | 20.7 GPa @Temperature 121 °C |
3000 ksi @Temperature 250 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® P-650M Polyester Prepreg, 7781 E-Glass Reinforced Nelcote® P-650M is a polyester resin system suitable for coating on any MIL-C-9084. P-650M has good electrical and mechanical properties and has been used in a wide variety of applications, includi.. |
|||
Compressive Modulus | 20.7 GPa @Temperature 24.0 °C |
3000 ksi @Temperature 75.2 °F |
|
Hexcel® HexPly® F155 Epoxy Resin, 120 Glass Fabric Hexcel designation: 120-38"-F155; Fiber: 450-1/2Information provided by HexCel |
|||
Compressive Modulus | 20.7 GPa @Temperature 71.0 °C |
3000 ksi @Temperature 160 °F |
|
Hexcel® HexPly® F155 Epoxy Resin, 220 Glass Fabric Information provided by HexCel |