Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.00236 GPa @Strain 10.0 % |
0.342 ksi @Strain 10.0 % |
|
Vicone High Performance Rubber VicoSilâ„¢ 909E-BK High Performance Silicone Rubber Information provided by Vicone |