Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 2.50 - 3.50 MPa @Temperature 1000 °C |
363 - 508 psi @Temperature 1830 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE 1.2.4. MIX GM Refractory Insulating Castable Description: This light weight gunning castable is composed of 1 part cement, 2 parts light weight grains and 4 parts vermiculite. Special additives provide for higher strength and less shrinkage.Re.. |
|||
Compressive Strength | 2.50 - 3.50 MPa @Temperature 100 °C |
363 - 508 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE 1.2.4. Mix Refractory Insulating Castable Description: This lightweight castable is composed of 1 part cement, 2 parts light weight grains and 4 parts vermiculite. Special additives provide for higher strength and less shrinkage.Remarks: Th.. |
|||
Compressive Strength | 2.50 - 3.50 MPa @Temperature 100 °C |
363 - 508 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE 95 Refractory Insulating Castable Description: Golite 95 is widely applied as an insulating backlining behind a dense castable, especially in the petrochemical industry.Remarks: These values apply to cast products. Also available in.. |