Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 1.77 - 3.43 MPa @Temperature 1000 °C, Time 10800 sec |
256 - 498 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories GUN-120L Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 2.45 - 3.43 MPa @Temperature 110 °C, Time 86400 sec |
356 - 498 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories MIX-2 Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |