Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.800 - 1.20 MPa @Temperature 100 °C |
116 - 174 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE 1.0.6. Mix Refractory Insulating Castable Description: This castable is composed of a high quality alumina cement and vermiculite and is applied as a backlining. Special additives are responsible for the low shrinkage. This castable can be .. |
|||
Compressive Strength | 0.800 - 1.20 MPa @Temperature 1000 °C |
116 - 174 psi @Temperature 1830 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE 1.0.6. Mix Refractory Insulating Castable Description: This castable is composed of a high quality alumina cement and vermiculite and is applied as a backlining. Special additives are responsible for the low shrinkage. This castable can be .. |