Mechanical Properties Metric English Comments
Compressive Strength 4.41 MPa

@Temperature 110 °C
640 psi

@Temperature 230 °F
Cold Crushing
Sharadaa Ceramics REFINSUL 11LI Insulating Castables Medium/High Purity
Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan..
Compressive Strength 4.41 MPa

@Temperature 1300 °C
640 psi

@Temperature 2370 °F
Cold Crushing
Sharadaa Ceramics Sharada LTM 1.0 Insulating Castable
Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd.
Compressive Strength 4.41 MPa

@Temperature 1300 °C
640 psi

@Temperature 2370 °F
Cold Crushing
Sharadaa Ceramics REFINSUL 13LI Insulating Castables Medium/High Purity
Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan..