Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 359 MPa @Temperature 177 °C |
52000 psi @Temperature 350 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® E-720 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-720 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-720 has a proven history in many demanding aerospac.. |
|||
Compressive Strength | 359 MPa @Temperature 216 °C |
52000 psi @Temperature 420 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® E-720 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-720 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-720 has a proven history in many demanding aerospac.. |
|||
Compressive Strength | 359 MPa @Temperature 93.3 °C |
52000 psi @Temperature 200 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 120 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Compressive Strength | 359 MPa @Temperature 93.3 °C |
52000 psi @Temperature 200 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Compressive Strength | 359 MPa @Temperature 82.2 °C |
52000 psi @Temperature 180 °F |
Wet; Vacuum/Oven Cured; SACMA 1-94 |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Compressive Strength | 359 MPa @Temperature 288 °C |
52000 psi @Temperature 550 °F |
Dry |
Renegade Materials Corporation MVK-14 Polyimide FreeForm™ Astroquartz 4581 Fabric MVK-14 Polyimide Astroquartz and S2 glass prepregs are an affordable, easy-to-process material for high-temperature radome and antenna applications. MVK-14 is a non-MDA alternative to BMI, cyanate e.. |