Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.280 MPa @Strain 50.0 % |
40.6 psi @Strain 50.0 % |
ISO 844 |
BASF Neopolen® P 9035 0.035 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9035 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9035.Note: In order to mea.. |
|||
Compressive Strength | 0.280 MPa @Strain 50.0 % |
40.6 psi @Strain 50.0 % |
ISO 844 |
BASF Neopolen® P 9335 MG 0.035 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9333 MG is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9333 MG.Note: In order .. |
|||
Compressive Strength | 0.280 MPa @Strain 50.0 % |
40.6 psi @Strain 50.0 % |
ISO 844 |
BASF Neopolen® P 9235 0.035 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea.. |
|||
Compressive Strength | 0.280 MPa @Strain 50.0 % |
40.6 psi @Strain 50.0 % |
ISO 844 |
BASF Neopolen® P 9435 0.035 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9435 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9435.Note: In order to mea.. |