Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 24.5 MPa @Strain 1.00 % |
3550 psi @Strain 1.00 % |
ASTM D695 |
Daelim H&L Plavis-C CM Conductive Polyimide Bearing Compression Molded. Plavis-C: Conductive, Electrical conductive, high thermal resistance and superior mechanical properties. Surface resistivity 10²-10³ OhmGeneral Plavis information for all grad.. |
|||
Compressive Strength | 24.5 MPa @Strain 1.00 % |
3550 psi @Strain 1.00 % |
ASTM D695 |
Daelim H&L Plavis-ESD CM Polyimide Bearing Compression Molded. Plavis-ESD: Electrostatic dissipative, Electrostatic dissipative, high thermal resistance and superior mechanical properties. And surface resistivity 10²-10³ OhmGeneral Plavis.. |
|||
Compressive Strength | 24.5 MPa @Strain 1.00 % |
3550 psi @Strain 1.00 % |
ASTM D695 |
Daelim H&L Plavis-G40 DF 40% Graphite Filled Aromatic Polyimide Bearing Direct Formed. Plavis-G-40: Graphite 40 wt% filled, Self lubricating grade with low thermal expansion.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 carbons is.. |
|||
Compressive Strength | 24.5 MPa @Strain 1.00 % |
3550 psi @Strain 1.00 % |
ASTM D695 |
Daelim H&L Plavis-N CM Unfilled Aromatic Polyimide Bearing Compression Molded. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS po.. |
|||
Compressive Strength | 24.5 MPa @Strain 1.00 % |
3550 psi @Strain 1.00 % |
ASTM D695 |
Daelim H&L Plavis-N DF Unfilled Aromatic Polyimide Bearing Direct Formed. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS polyimi.. |
|||
Compressive Strength | 24.5 MPa @Strain 1.00 % |
3550 psi @Strain 1.00 % |
ASTM D695 |
Daelim H&L Plavis-N ISO Unfilled Aromatic Polyimide Bearing Isostatically Molded. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS .. |