Mechanical Properties Metric English Comments
Compressive Strength 1.77 MPa

@Temperature 200 °C
256 psi

@Temperature 392 °F
Cold Crushing
Sharadaa Ceramics Sharada LTM 0.6 Insulating Castable
Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd.
Compressive Strength 1.77 MPa

@Temperature 200 °C
256 psi

@Temperature 392 °F
Cold Crushing
Sharadaa Ceramics Sharada LTM 0.7 Insulating Castable
Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd.
Compressive Strength 1.77 - 3.43 MPa

@Temperature 1000 °C,
Time 10800 sec
256 - 498 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories GUN-120L Light-Weight Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).