Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 11.0 MPa @Strain 1 % |
1600 psi @Strain 1 % |
ISO 604 |
Quadrant EPP Fluorosint® MT-01 PTFE + additives, enhanced grade, compression moulded (ISO Data) Fluorosint MT-01 is an extreme service grade developed specifically for applications where the benefits of PTFE-based materials also require strength, stiffness and stability. Fluorosint MT-01 deliv.. |
|||
Compressive Strength | 11.0 MPa @Strain 2 % |
1600 psi @Strain 2 % |
ISO 604 |
Quadrant EPP TIVAR® 1000 antistatic PE-UHMW + carbon black (ISO Data) By incorporating an effective carbon black grade, TIVAR 1000 antistatic offers the electrostatic dissipative properties often required for PE-UHMW components operating at high line speeds and convey.. |
|||
Compressive Strength | 11.0 MPa @Strain 2 % |
1600 psi @Strain 2 % |
ISO 604 |
Quadrant EPP TIVAR® Burnguard PE-UHMW + flame retardant + other additives (ISO Data) TIVAR Burnguard is a PE-UHMW grade containing a very effective non-halogenated flame retardant. Specifically developed to improve the poor flammability behaviour of straight forward virgin polyethyl.. |
|||
Compressive Strength | 11.0 MPa @Strain 2 % |
1600 psi @Strain 2 % |
ISO 604 |
Quadrant EPP TIVAR® Ceram P PE-UHMW + micro glass beads + other additives (ISO Data) TIVAR Ceram P is a wear improved PE-UHMW material with incorporated micro glass beads, specifically developed for use in the dewatering zone of paper machinery equipped with plastic wires and manufa.. |
|||
Compressive Strength | 11.0 MPa @Strain 2 % |
1600 psi @Strain 2 % |
ISO 604 |
Quadrant EPP TIVAR® ECO PE-UHMW reprocessed (ISO Data) This grade, partially composed of reprocessed PE-UHMW material, has an overall lower property level than the virgin TIVAR 1000 and a lower cost. Compared with virgin PE 500, however, it has a much b.. |
|||
Compressive Strength | 11.0 - 17.0 MPa @Temperature 1400 °C |
1600 - 2470 psi @Temperature 2550 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE 160 GM Refractory Insulating Castable Description: Golite 180 GM is a gunning mix that can be used up to very high temperatures in reducing conditions.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast. |