Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.91107 MPa @Strain 75.0 % |
132.14 psi @Strain 75.0 % |
ASTM D3575 |
Sekisui PIOCELAN LSP-20D Moldable Polymer Foam A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica.. |