Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 88.3 MPa @Temperature 150 °C |
12800 psi @Temperature 302 °F |
JIS K7208 |
Mitsui AURUM® JGN3030 Thermoplastic Polyimide Resin, Amorphous
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Compressive Strength | 88.3 MPa @Temperature 110 °C |
12800 psi @Temperature 230 °F |
Cold Crushing |
Sharadaa Ceramics REFCAST A SUPER High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Compressive Strength | 88.3 MPa @Temperature 110 °C |
12800 psi @Temperature 230 °F |
Cold Crushing |
Sharadaa Ceramics REFCAST LC60ABR Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Compressive Strength | 88.3 MPa @Temperature 1400 °C |
12800 psi @Temperature 2550 °F |
Cold Crushing |
Sharadaa Ceramics Sharada RFC-95 Gel Bonded Castables Mullite Bonded Free Flowing Cement Free Versatile Castable SystemProduct Characteristics: High Mullitisation, Free from Low Temperature eutectics, Non wetting to molten metals Ferrous/Non Ferrous, E.. |
|||
Compressive Strength | 88.3 MPa @Temperature 1500 °C |
12800 psi @Temperature 2730 °F |
Cold Crushing |
Sharadaa Ceramics ZAP 001 Smart Cast Application Special Properties: Thermal Shock Slag ResistanceIndustry: FoundryApplication Areas: Foundry LaddleInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Compressive Strength | 88.3 MPa @Temperature 1500 °C |
12800 psi @Temperature 2730 °F |
Cold Crushing |
Sharadaa Ceramics ZAP 006 Smart Cast Application Special Properties: Thermal Shock, Flame ErosionIndustry: Multi PurposeApplication: Burner Blocks all types of Thermal Shock ApplicationsInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Compressive Strength | 88.3 MPa @Temperature 1500 °C |
12800 psi @Temperature 2730 °F |
Cold Crushing |
Sharadaa Ceramics ZAP 008 Smart Cast Application Special Properties: Thermal Shock Slag ResistanceIndustry: SteelApplication: Pig Iron Laddle Safety Layer, Sponge Iron Rotary Kiln BackupInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Compressive Strength | 88.3 MPa @Temperature 1500 °C |
12800 psi @Temperature 2730 °F |
Cold Crushing |
Sharadaa Ceramics ZAP 009 Smart Cast Application Special Properties: Thermal Shock, Lesser Dross Formation, Non-wetting To AluminumIndustry: Non-FerrousApplication: Aluminum Melting/Holding Furnace, Launders, Risers, Transfer LaddlesInformation pr.. |
|||
Compressive Strength | 88.3 MPa @Temperature 1100 °C |
12800 psi @Temperature 2010 °F |
Cold Crushing |
Sharadaa Ceramics ZAP 011 Smart Cast Application Special Properties: Thermal Shock, Accretion, Co, Impact ResistanceIndustry: Sponge IronApplication: Sponge Rotary KilnInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Compressive Strength | 88.3 MPa @Temperature 1500 °C |
12800 psi @Temperature 2730 °F |
Cold Crushing |
Sharadaa Ceramics ZAP 012 Smart Cast Application Special Properties: Patching At Hot Conditions, Easy InstallationIndustry: All IndustryApplication: All type of Rotary Kilns, AL/CU Melting Furnaces, Rolling Mills, Forgoing Furnaces, IncineratorsIn.. |
|||
Compressive Strength | 88.3 MPa @Temperature 110 °C, Time 86400 sec |
12800 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories HSC-16H-W2 Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 88.3 MPa @Temperature 1000 °C, Time 10800 sec |
12800 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories HSC-16SF-W2 Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 88.3 MPa @Temperature 1000 °C, Time 10800 sec |
12800 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories HSC-18 Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 88.3 MPa @Temperature 1500 °C, Time 10800 sec |
12800 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories MMCT-75 Special Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 88.3 MPa @Temperature 1400 °C, Time 10800 sec |
12800 psi @Temperature 2550 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories SCX-16KL Special SiC Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 88.3 MPa @Temperature 800 °C, Time 10800 sec |
12800 psi @Temperature 1470 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories SCX-70 I Special SiC Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 88.3 MPa @Temperature 800 °C, Time 10800 sec |
12800 psi @Temperature 1470 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories SCX-85 I Special SiC Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 88.3 MPa @Temperature 1000 °C, Time 10800 sec |
12800 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories SFC-70 SiC Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 88.3 MPa @Temperature 1000 °C, Time 10800 sec |
12800 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories SFC-90S High-Alumina Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 88.3 MPa @Temperature 149 °C |
12800 psi @Temperature 300 °F |
JIS K7208 |
Mitsui AURUM® JGN3030 Polyimide, Glass Fiber Filled
(discontinued **) AURUM JGN3030 is a high performance thermoplastic polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, glass fiber .. |