Polymer Property : Compressive Strength = 115 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 0.790 MPa

@Strain 10.0 %
115 psi

@Strain 10.0 %
ISO 844
BASF Neopolen® P 9280 0.11 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9280 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9280.Note: In order to mea..
Compressive Strength 0.790 MPa

@Strain 10.0 %
115 psi

@Strain 10.0 %
ISO 844
BASF Neopolen® P 9270 0.11 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9270 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9270.Note: In order to mea..