Mechanical Properties Metric English Comments
Compressive Strength 7.00 MPa

@Strain 1 %
1020 psi

@Strain 1 %
ISO 604
Quadrant EPP TIVAR® 1000 antistatic PE-UHMW + carbon black (ISO Data)
By incorporating an effective carbon black grade, TIVAR 1000 antistatic offers the electrostatic dissipative properties often required for PE-UHMW components operating at high line speeds and convey..
Compressive Strength 7.00 MPa

@Strain 1 %
1020 psi

@Strain 1 %
ISO 604
Quadrant EPP TIVAR® 1000 ASTL PE-UHMW + specific additives (ISO Data)
TIVAR 1000 ASTL, based on a PE-UHMW grade with extremely high molecular weight, has been specifically developed for tough anti-abrasion applications. TIVAR 1000 ASTL shows a higher wear and abrasion..
Compressive Strength 7.00 MPa

@Strain 1 %
1020 psi

@Strain 1 %
ISO 604
Quadrant EPP TIVAR® Burnguard PE-UHMW + flame retardant + other additives (ISO Data)
TIVAR Burnguard is a PE-UHMW grade containing a very effective non-halogenated flame retardant. Specifically developed to improve the poor flammability behaviour of straight forward virgin polyethyl..
Compressive Strength 7.00 MPa

@Strain 1 %
1020 psi

@Strain 1 %
ISO 604
Quadrant EPP TIVAR® Ceram P PE-UHMW + micro glass beads + other additives (ISO Data)
TIVAR Ceram P is a wear improved PE-UHMW material with incorporated micro glass beads, specifically developed for use in the dewatering zone of paper machinery equipped with plastic wires and manufa..
Compressive Strength 7.00 MPa

@Strain 1 %
1020 psi

@Strain 1 %
ISO 604
Quadrant EPP TIVAR® ECO PE-UHMW reprocessed (ISO Data)
This grade, partially composed of reprocessed PE-UHMW material, has an overall lower property level than the virgin TIVAR 1000 and a lower cost. Compared with virgin PE 500, however, it has a much b..
Compressive Strength 7.00 MPa

@Strain 1 %
1020 psi

@Strain 1 %
ISO 604
Quadrant EPP TIVAR® MD PE-UHMW + metal detectable additive (ISO Data)
This PE-UHMW grade with extremely high degree of polymerisation contains a metal detectable additive which does hardly affect the inherent PE-UHMW key properties. TIVAR MD presents excellent toughne..
Compressive Strength 7.00 - 17.0 MPa

@Temperature 1000 °C
1020 - 2470 psi

@Temperature 1830 °F
Cold Crushing Strength
Gouda Vuurvast CURON 120 Dense Refractory Castable
Description: A general purpose castable for use up to 1200°C under normal operating conditions. Curon 120 has good thermal shock resistance.Remarks: These values apply to cast products. Also avai..
Compressive Strength 7.00 - 13.0 MPa

@Temperature 100 °C
1020 - 1890 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 145 P Dense Refractory Castable
Description: This material with an extreme plasticity is well suited for repair work or application as a thin layer.Remarks: These values apply to cast products.Information provided by Gouda Vuurvas..
Compressive Strength 7.00 - 13.0 MPa

@Temperature 1400 °C
1020 - 1890 psi

@Temperature 2550 °F
Cold Crushing Strength
Gouda Vuurvast CURON 145 P Dense Refractory Castable
Description: This material with an extreme plasticity is well suited for repair work or application as a thin layer.Remarks: These values apply to cast products.Information provided by Gouda Vuurvas..
Compressive Strength 7.00 - 13.0 MPa

@Temperature 1000 °C
1020 - 1890 psi

@Temperature 1830 °F
Cold Crushing Strength
Gouda Vuurvast GOLITE 130 GM Refractory Insulating Castable
Description: Golite 130 GM is a standard, medium weight gunning castable, combining a good mechanical strength with a low density and a low thermal conductivity.Remarks: These values apply to cast p..
Compressive Strength 7.00 - 13.0 MPa

@Temperature 1000 °C
1020 - 1890 psi

@Temperature 1830 °F
Cold Crushing Strength
Gouda Vuurvast GOLITE 130 Refractory Insulating Castable
Description: Golite 130 is a standard, medium weight castable, combining a good mechanical strength with a low density and a low thermal conductivity.Remarks: These values apply to cast products. Al..
Copyright © lookpolymers.com All Rights Reserved