Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 65.0 MPa @Strain 2 % |
9430 psi @Strain 2 % |
ISO 604 |
Quadrant EPP Techtron® HPV PPS + solid lubricant, bearing grade, extruded (ISO Data) As a reinforced, internally lubricated PPS grade, Techtron HPV PPS demonstrates an excellent combination of properties including wear resistance, load-bearing capabilities and dimensional stability .. |
|||
Compressive Strength | 65.0 MPa @Temperature 120 °C |
9430 psi @Temperature 248 °F |
ISO 604 |
Victrex® PEEK 450FE20 Polyetheretherketone, 20% PTFE Product Description:High performance thermoplastic material, 20% filled with PTFE Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA foo.. |
|||
Compressive Strength | 65.0 MPa @Temperature 200 °C |
9430 psi @Temperature 392 °F |
ISO 604 |
Victrex® PEEK 90GL60 Polyetheretherketone, 60% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 60% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, standard flow, FDA food contac.. |
|||
Compressive Strength | 65.0 MPa @Temperature 250 °C |
9430 psi @Temperature 482 °F |
ISO 604 |
Victrex® PEEK -HT™ 22CA30 PolyEtherKetone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact com.. |
|||
Compressive Strength | 65.0 MPa @Temperature 250 °C |
9430 psi @Temperature 482 °F |
ISO 604 |
Victrex® ST™ ST45CA30 PolyEtherKetoneEtherKetoneKetone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, .. |
|||
Compressive Strength | 65.0 MPa @Temperature 200 °C |
9430 psi @Temperature 392 °F |
ISO 604 |
Victrex® WG101™ Polyaryletherketone Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, black, granules for injection moulding, easy flow with wear additivesWG101 does not contai.. |
|||
Compressive Strength | 65.0 - 75.0 MPa @Temperature 100 °C |
9430 - 10900 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURASBOND 85 Moldable Refractory Material Description: Curasbond 85 is a pouring repairmass, characterized by excellent resistance to aluminum and rapid hardening. The product is supplied in two components: a dry powder and a liquid. It can.. |
|||
Compressive Strength | 65.0 - 75.0 MPa @Temperature 1000 °C |
9430 - 10900 psi @Temperature 1830 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 150 AC Dense Refractory Castable Description: Curon 150 AC is a coarse castable for use up to 1500°C with a high strength.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast. |
|||
Compressive Strength | 65.0 - 75.0 MPa @Temperature 100 °C |
9430 - 10900 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 150 HS Dense Refractory Castable Description: Dense refractory castableRemarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information provided by Gouda Vuurvast. |
|||
Compressive Strength | 65.0 - 75.0 MPa @Temperature 100 °C |
9430 - 10900 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 150 RN Dense Refractory Castable Description: This on sintered bauxite and low-iron alumina cement based castable contains stainless steel fibers, what results in a very good mechanical strength.Remarks: These values apply to cast .. |
|||
Compressive Strength | 65.0 - 75.0 MPa @Temperature 100 °C |
9430 - 10900 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 160 HF Dense Refractory Castable Description: This castable has a high volume stability and keeps its strength up to high temperatures. In addition, Curon 160 HF has an excellent thermal shock resistance. It is largely used in the .. |
|||
Compressive Strength | 65.0 - 75.0 MPa @Temperature 100 °C |
9430 - 10900 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast FLUCON 150 Dense Self Flowing Refractory Castable Description: Flucon 150 is a self-flowing low cement castable based on sintered bauxite.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast. |
|||
Compressive Strength | 65.0 - 75.0 MPa @Temperature 100 °C |
9430 - 10900 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast FLUCON 160 K Dense Self Flowing Refractory Castable Description: Flucon 160 K is a self-flowing low cement castable based on silicon carbide. This castable is characterized by high strength high abrasion resistance and excellent thermal shock resista.. |
|||
Compressive Strength | 65.0 - 75.0 MPa @Temperature 100 °C |
9430 - 10900 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 130 Dense Vibrating Refractory Castable Description: Vibron 130 is a vibrating castable with a low cement content, based on abrasion resistant spinel grains.Remarks: Indicated values apply to vibrated products.Information provided by Goud.. |
|||
Compressive Strength | 65.0 - 75.0 MPa @Temperature 100 °C |
9430 - 10900 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 13 S Dense Refractory Castable Description: Curon 13 S is a spinel based castable with a very low silica content and therefore it is suitable for direct contact with all kinds of aluminum/alloys and fluxes in aluminum melting/hol.. |
|||
Compressive Strength | 65.0 - 75.0 MPa @Temperature 100 °C |
9430 - 10900 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 160 HS Dense Refractory Castable Description: Because of the selection of raw materials, this castable has a high volume stability and a high strength up to high temperatures. In addition, Curon 160 HS has an excellent thermal shoc.. |
|||
Compressive Strength | 65.0 - 75.0 MPa @Temperature 100 °C |
9430 - 10900 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 160 HSC Dense Refractory Castable Description: Curon 160 HSC is a coarse abrasion resistant castable to be used up to 1600°C in reducing conditions.Remarks: These values apply to cast products.Information provided by Gouda Vuurva.. |
|||
Compressive Strength | 65.0 - 75.0 MPa @Temperature 100 °C |
9430 - 10900 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 160 K 50 Dense Vibrating Refractory Castable Description: Vibron 160 K 50 is a low cement castable based on silicon carbide and characterized by a very good thermal conductivity, high abrasion resistance and a good oxidation resistance up to 1.. |
|||
Compressive Strength | 65.0 - 75.0 MPa @Temperature 100 °C |
9430 - 10900 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 160 K Dense Vibrating Refractory Castable Description: Vibron 160 K is a low cement castable based on silicon carbide and characterized by a very good thermal conductivity and high abrasion resistance. The thermal shock resistance is excell.. |
|||
Compressive Strength | 65.0 - 75.0 MPa @Temperature 100 °C |
9430 - 10900 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 162 K Sp Dense Vibrating Refractory Silicon Carbide Castable Vibron 162 K Sp is a low cement castable based on silicon carbide. This castable is characterized by a very good thermal conductivity, a high abrasion resistance and high resistance against oxidatio.. |
|||
Compressive Strength | 65.0 - 75.0 MPa @Temperature 100 °C |
9430 - 10900 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 180 RAPID Dense Vibrating Refractory Castable Description: Vibron 180 Rapid is a low cement castable based on corundum with a special addition to enable a faster heating schedule. The material is supplied in two components. The B component cont.. |
|||
Compressive Strength | 65.0 MPa @Temperature 1000 °C |
9430 psi @Temperature 1830 °F |
Cold Crushing |
Sharadaa Ceramics VELECRETE RC 103 Rodding Castables Description: The Rodding Castables offered by us are user friendly in nature and does not require high energy mixing machines and vibrators. Free flowing in nature, these castables are designed in c.. |
|||
Compressive Strength | 65.0 MPa @Temperature 120 °C |
9430 psi @Temperature 248 °F |
ISO 604 |
Victrex® PEEK 650G Polyetheretherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta.. |
|||
Compressive Strength | 65.0 - 75.0 MPa @Temperature 100 °C |
9430 - 10900 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast FLUCON 160 H Dense Self Flowing Refractory Castable Description: Flucon 160 H is a self-flowing low cement castable on high fired high alumina grog base, characterized by a high strength and good thermal shock resistance.Remarks: These values apply t.. |