Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 46.0 MPa @Strain 1 % |
6670 psi @Strain 1 % |
ISO 604 |
Quadrant EPP Ketron® HPV PEEK + carbon fibres + PTFE + graphite, bearing grade, extruded (ISO Data) The addition of carbon fibres, PTFE and graphite to virgin PEEK results in a Ketron PEEK “bearing grade”. Its excellent tribological properties (low friction, long wear and high pressure-velocity .. |