Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 36.8 MPa @Temperature 1100 °C |
5330 psi @Temperature 2010 °F |
Cold Crushing |
Sharadaa Ceramics REFCAST 80 High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |