Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 340 MPa @Temperature 23.0 °C |
49300 psi @Temperature 73.4 °F |
|
Elisto THERMOSTAR® 4000 Mold Insulation Material Insulation of clamping platesInformation provided by elisto |
|||
Compressive Strength | 340 MPa @Temperature 23.0 °C |
49300 psi @Temperature 73.4 °F |
|
Elisto THERMOSTAR® LC 6000 Insulation Material Pattern material. Insulation materials for mechanical engineering.Information provided by elisto |