Mechanical Properties Metric English Comments
Compressive Strength 324 MPa

@Temperature 71.1 °C
47000 psi

@Temperature 160 °F
Wet; ASTM D695
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 120 E-Glass Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Compressive Strength 324 MPa

@Temperature 71.1 °C
47000 psi

@Temperature 160 °F
Wet; ASTM D695
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Compressive Strength 324 MPa

@Temperature 23.9 °C
47000 psi

@Temperature 75.0 °F
Dry; ASTM D695
Park Electrochemical Nelcote® P-650M Polyester Prepreg, 7781 E-Glass Reinforced
Nelcote® P-650M is a polyester resin system suitable for coating on any MIL-C-9084. P-650M has good electrical and mechanical properties and has been used in a wide variety of applications, includi..
Compressive Strength 324 MPa

@Temperature 288 °C
47000 psi

@Temperature 550 °F
Dry
Renegade Materials Corporation MVK-14 Polyimide FreeForm™ S2-Glass Fabric
MVK-14 Polyimide Astroquartz and S2 glass prepregs are an affordable, easy-to-process material for high-temperature radome and antenna applications. MVK-14 is a non-MDA alternative to BMI, cyanate e..