Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 230 MPa @Temperature 120 °C |
33400 psi @Temperature 248 °F |
ISO 604 |
Victrex® PEEK 450CA40 Polyetheretherketone, 40% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 40% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |
|||
Compressive Strength | 230 MPa @Temperature 23.0 °C |
33400 psi @Temperature 73.4 °F |
ISO 604 |
Victrex® PEEK 90GL60 Polyetheretherketone, 60% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 60% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, standard flow, FDA food contac.. |
|||
Compressive Strength | 230 MPa @Temperature 23.0 °C |
33400 psi @Temperature 73.4 °F |
ISO 604 |
Victrex® WG101™ Polyaryletherketone Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, black, granules for injection moulding, easy flow with wear additivesWG101 does not contai.. |