Polymer Property : Compressive Strength = 23.4 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 23.4 MPa

@Temperature 204 °C
3390 psi

@Temperature 399 °F
ASTM D 695
Saint-Gobain Meldin® 1003 Thermoplastic Bearing Material
Meldin 1003 components offer the highest level of strength and rigidity for this product family. They maintain high chemical, tensile, and flexural properties even at elevated temperatures.MeldinÂ..
Compressive Strength 23.4 MPa

@Temperature 1260 °C
3390 psi

@Temperature 2300 °F
Cold Crush Strength
BNZ Materials Blazecrete 2500 HS Dense Castable
Blazecrete 2500 HSis a high-duty castable designed to withstand loads and resist normal abrasion and erosion at moderate temperatures to 2500°F (1371°C). Use with Blaz 2100 for a dual component li..