Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 160 MPa @Temperature 120 °C |
23200 psi @Temperature 248 °F |
ISO 604 |
Victrex® PEEK 150GL30 30% Glass Fiber Reinforced Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact c.. |
|||
Compressive Strength | 160 MPa @Temperature 120 °C |
23200 psi @Temperature 248 °F |
ISO 604 |
Victrex® PEEK 450GL30 30% Glass Fiber Reinforced Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, F.. |
|||
Compressive Strength | 160 MPa @Temperature 120 °C |
23200 psi @Temperature 248 °F |
Result based on 450GL30; ISO 604 |
Victrex® PEEK 450GL30 Polyetheretherketone, 30% Glass Fiber, Black Product Description: High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, Standard viscos.. |
|||
Compressive Strength | 160 MPa @Temperature 120 °C |
23200 psi @Temperature 248 °F |
ISO 604 |
Victrex® PEEK 90GL30 BLACK EU 30% Glass Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, FDA and EU food contact compliant, .. |
|||
Compressive Strength | 160 MPa @Temperature 120 °C |
23200 psi @Temperature 248 °F |
ISO 604 |
Victrex® PEEK 90GL30 Polyetheretherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta.. |
|||
Compressive Strength | 160 MPa @Temperature 120 °C |
23200 psi @Temperature 248 °F |
ISO 604 |
Victrex® WG101™ Polyaryletherketone Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, black, granules for injection moulding, easy flow with wear additivesWG101 does not contai.. |
|||
Compressive Strength | 160 MPa @Temperature 120 °C |
23200 psi @Temperature 248 °F |
ISO 604 |
Victrex® PEEK 150GL30 Black Polyetheretherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact co.. |