Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 140 MPa @Strain 5 % |
20300 psi @Strain 5 % |
ISO 604 |
Quadrant EPP Ketron® 1000 PEEK unfilled, extruded (ISO Data) Ketron PEEK-1000 stock shapes are produced from virgin polyetheretherketone resin and offer the highest toughness and impact strength of all Ketron PEEK grades. Both Ketron PEEK-1000 natural & black.. |
|||
Compressive Strength | 140 MPa @Temperature 120 °C |
20300 psi @Temperature 248 °F |
ISO 604 |
Victrex® PEEK 90GL60 Polyetheretherketone, 60% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 60% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, standard flow, FDA food contac.. |
|||
Compressive Strength | 140 MPa @Temperature 23.0 °C |
20300 psi @Temperature 73.4 °F |
ISO 604 |
Victrex® PEEK -HT™ G22 PolyEtherKetone, Unreinforced Product Description:High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact complia.. |
|||
Compressive Strength | 140 MPa @Temperature 23.0 °C |
20300 psi @Temperature 73.4 °F |
Result based on HT G22; ISO 604 |
Victrex® HT™ G45 Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, low flow, FDA food contact complia.. |