Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 130 MPa @Strain 5 % |
18900 psi @Strain 5 % |
ISO 604 |
Quadrant EPP Duratron® PAI T4301 PAI + graphite + PTFE, extruded (ISO Data) The addition of PTFE and graphite provides higher wear resistance and lower coefficient of friction compared to the unfilled grade as well as a lower tendency to stick-slip. Duratron T4301 PAI also .. |
|||
Compressive Strength | 130 MPa @Strain 5 % |
18900 psi @Strain 5 % |
ISO 604 |
Quadrant EPP Duratron® PAI T4501 PAI + graphite + PTFE, compression moulded (ISO Data) Compression moulded Duratron T4501 PAI is similar in composition to Duratron T4301 PAI, and is selected when larger shapes are required Very high maximum allowable service temperature in air (250°C.. |
|||
Compressive Strength | 130 MPa @Temperature 23.0 °C |
18900 psi @Temperature 73.4 °F |
ISO 604 |
Victrex® PEEK 150G / 151G Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c.. |
|||
Compressive Strength | 130 MPa @Temperature 23.0 °C |
18900 psi @Temperature 73.4 °F |
ISO 604 |
Victrex® PEEK 150G903 Black Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact compliant, colou.. |
|||
Compressive Strength | 130 MPa @Temperature 23.0 °C |
18900 psi @Temperature 73.4 °F |
ISO 604 |
Victrex® PEEK 90G Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c.. |
|||
Compressive Strength | 130 MPa @Temperature 120 °C |
18900 psi @Temperature 248 °F |
ISO 604 |
Victrex® PEEK 450GL15 Polyetheretherketone, 15% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 15% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, F.. |