Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.0900 MPa @Strain 10.0 % |
13.1 psi @Strain 10.0 % |
DIN-EN 826 |
BASF E-por® 0.02 g/cc Density; Styrene and Ethylene (Europe) Description: Expandable granules made of styrene and ethylene containing polymers without flame retardant (blowing agent: pentane).Application: For the production of elastic, multi-shock absorbing e.. |
|||
Compressive Strength | 0.0900 MPa @Strain 10.0 % |
13.1 psi @Strain 10.0 % |
ISO 844 |
BASF Neopolen® P 8225 K 0.025 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 8225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8225 K.Note: In order to.. |