Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.650 GPa @Temperature 90.0 °C |
94.3 ksi @Temperature 194 °F |
|
LATI Latamid 66 PA 66 Polyamide 66 (PA66). Unfilled.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A. |
|||
Tensile Modulus | 0.650 GPa @Temperature 90.0 °C |
94.3 ksi @Temperature 194 °F |
|
LATI Latamid 6 H2PX-V0 PA 6, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am.. |
|||
Tensile Modulus | 0.650 GPa @Temperature 150 °C |
94.3 ksi @Temperature 302 °F |
|
LATI Latamid 68 H2-V0 PA6/PA66 copolymer, Heat Stabilized, Flame Retardant PA6/PA66 copolymer (PA6/PA66) based compound. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Good surface appearance.Availability: Africa & Middle Ea.. |
|||
Tensile Modulus | 0.650 GPa @Temperature 90.0 °C |
94.3 ksi @Temperature 194 °F |
|
LATI Latan 3E71 POM Polyoxymethylene (POM). Toughened. High viscosity. Good elongation and impact resistanceAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by .. |
|||
Tensile Modulus | 0.650 GPa @Temperature 90.0 °C |
94.3 ksi @Temperature 194 °F |
|
LATI Latene® 22H2 MX/25 PP Homopolymer, Heat Stabilized Polypropylene homopolymer (PPh) based compound. Heat stabilized. Special mineral filler. Very good surface appearance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A.. |
|||
Tensile Modulus | 0.650 GPa @Temperature 90.0 °C |
94.3 ksi @Temperature 194 °F |
|
LATI Latigray 53/22-01 CX/25 PP Homopolymer, Impact Modified Radiopaque compound based on Polypropylene homopolymer (PPh), impact modified. Special mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformatio.. |
|||
Tensile Modulus | 0.650 GPa @Temperature 90.0 °C |
94.3 ksi @Temperature 194 °F |
|
LATI Latene® 9H TES/30 PP Homopolymer, Heat Stabilized Polypropylene homopolymer (PPh) based compound. Heat stabilized. Aesthetic talc.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Tensile Modulus | 0.650 GPa @Temperature 90.0 °C |
94.3 ksi @Temperature 194 °F |
|
LATI Later 4 PBT Polybutylene Terephthalate (PBT). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A. |