Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 60.5 GPa @Temperature 177 °C |
8770 ksi @Temperature 351 °F |
|
Hexcel® HexPly® F263 Epoxy Resin, F3T584 Carbon Fabric Hexcel designation: F3T584-42"-F263; Fiber: T300 CelionInformation provided by HexCel |