Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.70 GPa @Temperature 23.0 °C |
537 ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® 79G13HSL BK039 Nylon 66
(Unverified Data**) Zytel® 79G13HSL BK039 is a 13 % glass reinforced, heat stabilized, lubricated slightly toughened black polyamide 66 for injection molding. It has improved impact resistance.Information provided by .. |
|||
Tensile Modulus | 3.70 GPa @Temperature 23.0 °C |
537 ksi @Temperature 73.4 °F |
|
LATI Larpeek 10 PEEK Polyetheretherketone (PEEK). Unfilled. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe;.. |
|||
Tensile Modulus | 3.70 GPa @Temperature 60.0 °C |
537 ksi @Temperature 140 °F |
|
LATI Larpeek 10 PEEK Polyetheretherketone (PEEK). Unfilled. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe;.. |
|||
Tensile Modulus | 3.70 GPa @Temperature 150 °C |
537 ksi @Temperature 302 °F |
|
LATI Latamid 6 H2 G/35 PA 6, 35% Glass Fiber Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibersAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Tensile Modulus | 3.70 GPa @Temperature 60.0 °C |
537 ksi @Temperature 140 °F |
|
LATI Latamid 66 H2E21 G/13 PA 66, 13% Glass Fiber Reinforced Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. Glass fibers. High impact resistance. Good impact resistance even at low temperature.Availability: Africa & Middle East; Asia Pacific;.. |
|||
Tensile Modulus | 3.70 GPa @Temperature 90.0 °C |
537 ksi @Temperature 194 °F |
|
LATI Lapex R G/10 PPSU, 10% Glass Reinforced Polyphenylene Sulfone (PPSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A.. |
|||
Tensile Modulus | 3.70 GPa @Temperature 23.0 °C |
537 ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® 79G13HSL NC010 Nylon 66
(Unverified Data**) Zytel® 79G13HSL is a 13% glass fiber reinforced, heat stabilized, lubricated slightly toughened polyamide 66 for injection molding. It has improved impact resistance.Information provided by DuPont .. |
|||
Tensile Modulus | 3.70 GPa @Temperature 120 °C |
537 ksi @Temperature 248 °F |
|
LATI Kelon® A H CEG/40 PA 66, Glass/Mineral Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers / Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati.. |