Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 32.0 GPa @Temperature 60.0 °C |
4640 ksi @Temperature 140 °F |
|
LATI Laramid K/40 HM PPA, 40% Carbon Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Carbon fiber. High tensile modulus. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; .. |
|||
Tensile Modulus | 32.0 GPa @Temperature 150 °C |
4640 ksi @Temperature 302 °F |
ISO 527-1 |
Vyncolit Neopreg Kinel® SK4502 S8 Carbon Reinforced Molding Compound KINEL SK4502 S8 is a long carbon fiber reinforced BMI molding compound suited for very demanding tribological applications, high speeds and temperatures even under dry running conditions. Thermal ex.. |