Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 27.6 GPa @Temperature 87.8 °C |
4000 ksi @Temperature 190 °F |
0° Direction, Dry; ASTM D638 Type 1 |
Park Electrochemical Nelcote® E-722 Epoxy Prepreg, 285 Kevlar® Reinforced Nelcote® E-722 is a modified 350°F cure epoxy system with excellent processing characteristics for vacuum bag, press, and autoclave molding.Key Features and Benefits:Epoxy resin system optimized f.. |
|||
Tensile Modulus | 27.6 GPa @Temperature 149 °C |
4000 ksi @Temperature 300 °F |
Dry; ASTM D638 |
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 581 Quartz Reinforced Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp.. |
|||
Tensile Modulus | 27.6 GPa @Temperature 71.0 °C |
4000 ksi @Temperature 160 °F |
1/2 hr |
Hexcel® HexPly® F515 Epoxy Resin, 7781 Glass Fabric Hexcel designation: 7781-38"-F515; Fiber 75-1/0Information provided by HexCel |