Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.75 GPa @Temperature 23.0 °C |
399 ksi @Temperature 73.4 °F |
5mm/min (0.2in/min); ASTM D638 |
DuPont Performance Polymers Delrin® 100AF Acetal Homopolymer
(Unverified Data**) Delrin® 100AF is a high viscosity acetal homopolymer containing 20% Teflon® PTFE fibers. It is designed for applications requiring low wear and/or low friction against steel, itself, and other pla.. |
|||
Tensile Modulus | 2.75 GPa @Temperature 90.0 °C |
399 ksi @Temperature 194 °F |
|
LATI Lapex A PES Polyether Sulfone (PES). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInf.. |