Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 26.9 GPa @Temperature 87.8 °C |
3900 ksi @Temperature 190 °F |
0° Direction, Wet (2hr water boil immersion); ASTM D638 Type 1 |
Park Electrochemical Nelcote® E-722 Epoxy Prepreg, 285 Kevlar® Reinforced Nelcote® E-722 is a modified 350°F cure epoxy system with excellent processing characteristics for vacuum bag, press, and autoclave molding.Key Features and Benefits:Epoxy resin system optimized f.. |
|||
Tensile Modulus | 26.9 GPa @Temperature 93.3 °C |
3900 ksi @Temperature 200 °F |
0° Direction, Dry; ASTM D638 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Tensile Modulus | 26.9 GPa @Temperature -53.9 °C |
3900 ksi @Temperature -65.0 °F |
0° Direction, Dry; Vacuum/Oven Cured; ASTM D3039-95 |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Tensile Modulus | 26.9 GPa @Temperature 71.0 °C |
3900 ksi @Temperature 160 °F |
|
Hexcel® HexPly® F155 Epoxy Resin, K285 Kevlar Fabric Information provided by HexCel |
|||
Tensile Modulus | 26.9 GPa @Temperature 23.0 °C |
3900 ksi @Temperature 73.4 °F |
|
Hexcel® HexPly® F650 Bismaleimide Resin with Quartz 581 fabric reinforcement Laminate Physicals: 55.4% Fiber volume, 31.4% Resin content, 0.7% Voids, 1.78% gm.cc Specific gravityInformation provided by HexCel |