Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 26.2 GPa @Temperature 93.3 °C |
3800 ksi @Temperature 200 °F |
0° Direction, Dry; ASTM D638 Type 1 |
Park Electrochemical Nelcote® E-722 Epoxy Prepreg, 285 Kevlar® Reinforced Nelcote® E-722 is a modified 350°F cure epoxy system with excellent processing characteristics for vacuum bag, press, and autoclave molding.Key Features and Benefits:Epoxy resin system optimized f.. |
|||
Tensile Modulus | 26.2 GPa @Temperature 23.9 °C |
3800 ksi @Temperature 75.0 °F |
0° Direction, Dry; ASTM D638 Type 1 |
Park Electrochemical Nelcote® P-600 Polyester Prepreg, 7781 E-Glass Reinforced Nelcote® P-600 is a general purpose 190°F curing polyester system widely accepted as a cost-effective alternative to wet lay-up processingKey Features and Benefits:Meets MIL-R-7575 requirements160.. |
|||
Tensile Modulus | 26.2 GPa @Temperature 23.9 °C |
3800 ksi @Temperature 75.0 °F |
Dry; ASTM D638 |
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 581 Quartz Reinforced Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp.. |