Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 12.0 GPa @Temperature -40.0 °C |
1740 ksi @Temperature -40.0 °F |
ISO 527 |
DuPont Performance Polymers Rynite® FR530 BK507 PET
(Unverified Data**) Rynite® FR530 BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 12.0 GPa @Temperature 23.0 °C |
1740 ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® 73G50HSLA BK416 Nylon 6
(Unverified Data**) Zytel® 73G50HSLA BK416 is a 50% glass fiber reinforced, heat stabilized, lubricated, polyamide 6 resin for injection molding. It has an excellent surface appearance and gloss.Information provided .. |
|||
Tensile Modulus | 12.0 GPa @Temperature 60.0 °C |
1740 ksi @Temperature 140 °F |
|
LATI Laramid G/35 PPA, 35% Glass Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Tensile Modulus | 12.0 GPa @Temperature 90.0 °C |
1740 ksi @Temperature 194 °F |
|
LATI Laramid G/45 PPA, 45% Glass Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Tensile Modulus | 12.0 GPa @Temperature 120 °C |
1740 ksi @Temperature 248 °F |
|
LATI Latamid 66 H2 K/50 PA 66, 50% Carbon Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl.. |
|||
Tensile Modulus | 12.0 GPa @Temperature 23.0 °C |
1740 ksi @Temperature 73.4 °F |
|
LATI Laramid G/30 PPA, 30% Glass Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Tensile Modulus | 12.0 GPa @Temperature 150 °C |
1740 ksi @Temperature 302 °F |
|
LATI Laramid K/40 HM PPA, 40% Carbon Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Carbon fiber. High tensile modulus. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; .. |
|||
Tensile Modulus | 12.0 GPa @Temperature 60.0 °C |
1740 ksi @Temperature 140 °F |
|
LATI Latigloss 66 H2 G/50 F2 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized Product with high mechanical properties and exceptional surface finish based on Polyamide 66 (PA66). Heat stabilized. Glass fibers. Potentially suitable for food/medical contact application. Availab.. |
|||
Tensile Modulus | 12.0 GPa @Temperature 23.0 °C |
1740 ksi @Temperature 73.4 °F |
|
LATI Latilon 28D K/20 PC, 20% Carbon Fiber Reinforced Polycarbonate (PC) based compound. Carbon fiber. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided b.. |
|||
Tensile Modulus | 12.0 GPa @Temperature 23.0 °C |
1740 ksi @Temperature 73.4 °F |
|
LATI Latiohm 66-06 PD03 G/20 PA66, 20% Glass Fiber Reinforced Semiconductive/dissipative product based on Polyamide 66 (PA66). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Tensile Modulus | 12.0 GPa @Temperature 23.0 °C |
1740 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® 70G35NOX BK309 Nylon 66 Zytel® 70G35NOX BK309 is a 35% glass reinforced, polyamide 66 resin developed for Selective Catalytic Reduction applications that require exposure to water/urea solution.Information provided by DuP.. |