Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 8.80 GPa @Temperature 23.0 °C |
1280 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® FE270038 BK267 Nylon 66
(Unverified Data**) Zytel® FE270038 is a 40% glass fiber/mineral reinforced, heat stabilized polyamid 66 for injection molding. It is well suited for water injection technology.Information provided by DuPont Performan.. |
|||
Tensile Modulus | 8.80 GPa @Temperature 23.0 °C |
1280 ksi @Temperature 73.4 °F |
|
LATI Latamid 6 H2 G/30 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla.. |
|||
Tensile Modulus | 8.80 GPa @Temperature 23.0 °C |
1280 ksi @Temperature 73.4 °F |
|
LATI Latamid SP1 G/30 PA 6.10, 30% Glass Fiber Reinforced Polyamide 6.10 (PA6.10) based compound. Glass fibers. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus.. |
|||
Tensile Modulus | 8.80 GPa @Temperature 23.0 °C |
1280 ksi @Temperature 73.4 °F |
|
LATI Latamid 66 H2 G/25-V0KB PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn.. |
|||
Tensile Modulus | 8.80 GPa @Temperature 23.0 °C |
1280 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66
(Unverified Data**) Zytel® 80G33HS1L BK104 is a 33% glass fiber reinforced, heat stabilized black polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Information provide.. |